Air quenched basic oxygen furnace steel slag (BOF-SS) is processed at very high cooling rate, which is expected to have different cementitious properties from conventional slowly cooled BOF-SS. For this purpose, the...Air quenched basic oxygen furnace steel slag (BOF-SS) is processed at very high cooling rate, which is expected to have different cementitious properties from conventional slowly cooled BOF-SS. For this purpose, the strength activity indexes of air quenched and slowly cooled BOF-SS are investigated. The results reveal that, under the specific surface area (S) of 490 m^2/kg, the compressive strength activity index reaches 1.24 after 28 days with replacement of 15% air quenched BOF-SS and reaches 1.05 after 28 days with replacement of 20% air quenched BOF-SS and 30%granulated blast furnace slag (GBFS). The cementitious activity of air quenched BOF-SS is obviously higher than that of slowly cooled BOF-SS, mainly because it contains more C3 S and glassy phases.展开更多
The desulfurization ability of refining slag with relative lower basicity (B) and Al2O3 content (B = 3.5-5.0; 20wt%-25wt% Al2O3) was studied. Firstly, the component activities and sulfide capacity (Cs) of the sl...The desulfurization ability of refining slag with relative lower basicity (B) and Al2O3 content (B = 3.5-5.0; 20wt%-25wt% Al2O3) was studied. Firstly, the component activities and sulfide capacity (Cs) of the slag were calculated. Then slag-metal equilibrium experiments were carried out to measure the equilibrium sulfur distribution (Ls). Based on the laboratorial experiments, slag composition was optimized for a better desulfurization ability, which was verified by industrial trials in a steel plant. The obtained results indicated that an MgO-saturated CaO-Al2O3-SiO2-MgO system with the basicity of about 3.5-5.0 and the Al2O3 content in the range of 20wt%-25wt% has high activity of CaO (αCaO), with no deterioration of Cs compared with conventional desulfurization slag. The measured Ls between high-strength low-alloyed (HSLA) steel and slag with a basicity of about 3.5 and an Al2O3 content of about 20wt% and between HSLA steel and slag with a basicity of about 5.0 and an Al2O3 content of about 25wt% is 350 and 275, respectively. The new slag with a basicity of about 3.5-5.0 and an Al2O3 content of about 20wt% has strong desulfurization ability. In particular, the key for high-efficiency desulfurization is to keep oxygen potential in the reaction system as low as possible, which was also verified by industrial trials.展开更多
基金Item Sponsored by National Natural Science Foundation of China(51234003)
摘要Air quenched basic oxygen furnace steel slag (BOF-SS) is processed at very high cooling rate, which is expected to have different cementitious properties from conventional slowly cooled BOF-SS. For this purpose, the strength activity indexes of air quenched and slowly cooled BOF-SS are investigated. The results reveal that, under the specific surface area (S) of 490 m^2/kg, the compressive strength activity index reaches 1.24 after 28 days with replacement of 15% air quenched BOF-SS and reaches 1.05 after 28 days with replacement of 20% air quenched BOF-SS and 30%granulated blast furnace slag (GBFS). The cementitious activity of air quenched BOF-SS is obviously higher than that of slowly cooled BOF-SS, mainly because it contains more C3 S and glassy phases.
基金financially supported by the National Basic Research Program of China (No. 2010CB630806)the State Key Laboratory of Advanced Metallurgy, University of Science and Technology Beijing (No. 41603015)
摘要The desulfurization ability of refining slag with relative lower basicity (B) and Al2O3 content (B = 3.5-5.0; 20wt%-25wt% Al2O3) was studied. Firstly, the component activities and sulfide capacity (Cs) of the slag were calculated. Then slag-metal equilibrium experiments were carried out to measure the equilibrium sulfur distribution (Ls). Based on the laboratorial experiments, slag composition was optimized for a better desulfurization ability, which was verified by industrial trials in a steel plant. The obtained results indicated that an MgO-saturated CaO-Al2O3-SiO2-MgO system with the basicity of about 3.5-5.0 and the Al2O3 content in the range of 20wt%-25wt% has high activity of CaO (αCaO), with no deterioration of Cs compared with conventional desulfurization slag. The measured Ls between high-strength low-alloyed (HSLA) steel and slag with a basicity of about 3.5 and an Al2O3 content of about 20wt% and between HSLA steel and slag with a basicity of about 5.0 and an Al2O3 content of about 25wt% is 350 and 275, respectively. The new slag with a basicity of about 3.5-5.0 and an Al2O3 content of about 20wt% has strong desulfurization ability. In particular, the key for high-efficiency desulfurization is to keep oxygen potential in the reaction system as low as possible, which was also verified by industrial trials.